EP28M-1 Product Description

Low Viscosity, Room Temperature Curing Two Component Epoxy Compound For High Performance Casting And Bonding

EP30-4 Product Information

EP30-4 Two Part Epoxy System

Optically Clear, Two Component Epoxy Adhesive for High Performance Bonding, Coating, Sealing and Casting Featuring Superior Non-Yellowing Properties, Low Viscosity and Rapid Curing.

EP38 Product Information

EP38 Two Component Epoxy

Two component epoxy for potting, bonding, sealing and coating

EP39-2 Product Information

EP39-2 Two Part Epoxy

Low Viscosity, Fast Curing, Two Component, High Performance Optical Epoxy for Bonding, Sealing, Coating and Casting Featuring Excellent Chemical Resistance.

EP39-2LV Product Description

EP39-2LV Two Component Epoxy

Low Viscosity, Fast Curing, Two High Performance Optical Epoxy For Bonding, Sealing, Coating & Casting Featuring Excellent Chemical Resistance

EP3FL Product Information

EP3FL One Part Epoxy Compound

One Component, Thermal Shock and Heat Resistant, Flexibilized Epoxy System for Bonding, as well as for Potting and Encapsulations up to ¼ Inch Thick; Features Good Toughness and Fast Cures.

EP3HT Product Information

EP3HT One Part Epoxy

One Component, Epoxy System for Bonding, Sealing and Coating Featuring Very Fast Cure along with High Shear Strength Properties.

EP3HTS Product Information

EP3HTS One Part Epoxy

One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed.

EP3HTSMed Product Information

EP3HTSMed One Part Medical Grade Epoxy

One Component, Heat Curing, Silver Filled, Electrically Conductive Epoxy Adhesive/Sealant Featuring High Shear Strength and Good Temperature Resistance Along With a Rapid Cure Speed

EP3RR-1 Product Description

EP3RR-1 One Part Epoxy

One Part, Lower Viscosity, Thermally Conductive Epoxy System for High Performance Potting, Encapsulation and Underfill Applications Featuring Exceptional Dimensional Stability and Rapid Curing at 230-250°F.