Master Bond has developed a wide variety of one and two component high peel strength adhesives for challenging bonding applications. Peel strength can be described as a material's ability to resist forces that can pull or peel it apart at a predetermined angle and rate.
Properties of Master Bond's High Peel Strength Adhesives
High peel strength epoxies provide excellent physical strength properties, toughness and resistance to vibration, impact and shock. Specific grades are also noted for:
- Low temperature serviceability
- Excellent adhesion to dissimilar substrates
- Withstanding exposure to thermal cycling
- Thermal and electrical conductivity
Master Bond offers a variety of adhesive systems with high peel strength properties.
Select Master Bond compositions feature both high peel and shear strength properties. For example two component, room temperature curing epoxy system EP31ND exhibits a tensile lap shear strength of 4,000-4,200 psi and a T-peel strength of >50 pli. In contrast single component no-mix epoxy adhesive Supreme 10HT has a tensile lap shear strength of 3,600-3,800 psi and a T-peel strength of >25-30 pli.
Some Popular High Peel Strength Adhesives, Sealants and Coatings
![]() |
EP21TDCHT High strength, high temperature resistant, two part system with excellent bond strength and thermal cycling capabilities. Serviceable from -100°F to +350°F. Meets MIL-STD-883J Section 3.5.2 for thermal stability. Moderate viscosity. Superior toughness. Withstands vibration, impact, shock. Good dimensional stability. Convenient one to one mix ratio. Dependable electrical insulation properties. |
![]() |
Supreme 10HT One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance. |
![]() |
EP21TDC-4 Two part, room temperature curing epoxy with outstanding flexibility and superb adhesion to many rubbers and metals. Excellent thermal cycling properties. Ability to withstand mechanical shock and vibration. T-peel strength 25-35 pli. Elongatio >200%. Water and chemical resistant. Operating temperature range -100°F to +250°F. |
![]() |
EP31ND Non-drip structural epoxy adhesive. Paste consistency. Gap filling. Unmatched peel and shear strength. Tough and resilient. Protects against exposure to water, oil, fuels. Cures at room temperature. Service temperature range from -60°F to +250°F. |
![]() |
EP40ND Excellent adhesion to metals and engineering plastics such as polycarbonates, acrylics. Flexible. For bonding, potting, sealing compound. High shear/peel strength. Resists mechanical shocks and vibration. Moderately low exotherm during cure. Serviceable from -100°F to +250°F. Paste consistency. |
![]() |
EP21TDC-2AN Flexibilized. Thermally conductive/electrically insulative. Thermal conductivity 22-24 BTU· in/ft2 hr· ° F. Serviceable from 4K to +250°F. Superb impact resistance. Long working life. High peel strength. Elongatio >25%. |
![]() |
EP72M4 Tough, resilient, room temperature curing epoxy adhesive. Resists exposure to vibration, impact and shock. Superior peel and shear strength. |