UV16 Product Information | MasterBond.com

Low viscosity, one component, UV curable epoxy based system

UV16 One Part UV Curable Compound

Key Features

  • Good physical strength properties
  • Low shrinkage upon curing
  • Cationic curing system, no oxygen inhibition
  • Passes NASA low outgassing tests