UV23FLDC-80 Product Information | MasterBond.com

One component, dual curing (UV light and heat) that cures with good flexibility

Key Features

  • Cures in shadowed out areas with heat
  • Curing temperature 80-85°C
  • Low viscosity, not thixotropic
  • Excellent elongation