EP35SP Type V Two Part Epoxy EP35SP Type V

Tough, high temperature resistant heat curing epoxy adhesive. Service temperature range from -80°F to +500°F. Durable, high strength bonds even after prolonged exposure to high temperatures. Ability to withstand thermal cycling and chemical exposure.

EP35TDC Two Part Epoxy EP35TDC

Tough, room temperature curing epoxy paste adhesive for high temperature bonding. Serviceable from -60°F to +450-500°F. Non-drip system. Gap filling. Resistant against thermal cycling and chemical exposure.

EP36 One Part B-Stage Epoxy EP36

One part B-staged epoxy. Flexibilized and toughened. Withstands rigorous thermal cycling and thermal shocks. Superb electrical insulation properties. Ideal for potting/encapsulation. Serviceable from -100°F to +500°F. Available in 30 gram cookies.

EP36CLV One Part Epoxy Compound EP36CLV

One component, B-staged epoxy. Features low viscosity and excellent electrical insulation properties. Operating service temperature range -100°F to +500°F. Combines flexibility and toughness. Superior chemical resistance to water, acids, bases, fuels and oils. Elongatio >50%.

EP36FR One Component Epoxy EP36FR

Flame retardant B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies.

EP37-3 Two Part Epoxy System EP37-3

Resilient, optically clear, two component epoxy resin system. Long working life. Excellent electrical insulation properties. Cures accelerated by heat. Chemically resistant. Low mixed viscosity. Serviceable from -80°F to +250°F. Two to one mix ratio by weight. Withstands impact.

EP37-3FLF Two Component Epoxy System EP37-3FLF

Highly flexible, low viscosity, optically clear adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume.

Two Part Epoxy EP37-3FLFAOND EP37-3FLFAOND

Highly flexible, low viscosity adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume.

EP37-3FLSP Two Component Epoxy EP37-3FLSP

Highly flexible. Low viscosity. Optically clear. Serviceable from 4K to +200°F. Superior dimensional stability. Long working life and low exotherm during curing. Ideal for large volume potting and casting. Excellent impact resistant.

EP37-3LV Two Part Epoxy System EP37-3LV

Clear, two component epoxy system has long pot life. Convenient one to one mix ratio. High bond strength. Superb chemical resistance properties. Used in bonding, sealing, potting and filament winding applications. Low viscosity compound. Exceptionally low exotherm. Cures rigid. Service operating temperature range from -60°F to +250°F.