EP77M-FMed Rapid room temperature curing silver filled electrically conductive adhesive. One to one mix ratio by weight or volume. Fixture time within 5-7 minutes even in small volumes. Exceptional low volume resistivity. Low outgassing. Superior bond strength to similar/dissimilar substrates. Serviceable from -60°F to +250°F. |
|
EP79 Cost effective alternative to silver filled epoxy with a silver coated nickel filler. Excellent conductivity and physical properties. Superior durability and thermal cycling capabilities. Cures readily at room temperature. Convenient one to one mix ratio weight or volume. Superb heat dissipation. Low linear shrinkage upon cure. Withstands 1,000 hours 85°C/85% RH. Serviceable from 4k to +275°F. Available in premixed and frozen syringes. |
|
EP79FL Highly flexible, silver coated/nickel filled epoxy system. T-peel greater than 20 pli. Low volume resistivity. High bond strength to similar and dissimilar substrates. Resists exposure to thermal cycling. Serviceable from 4k to +275°F. One to one mix ratio by weight. Ambient temperature curing. 100% reactive. Withstands moisture, chemical exposure. Available in premixed and frozen syringes. |
|
FL901S High performance, silver filled epoxy adhesive film system with outstanding electrical and thermal conductivity. Superior mechanical strength, convenient handling, good storage stability and fast cures at moderate temperatures. Specialty preforms are available. Serviceable from -100°F to +500°F. |
|
MasterSil 151S Addition curing, two part silicone for use as an adhesive, sealant, coating or form-in-place gasketing material. Despite its silicone chemistry, it passes NASA low outgassing specifications. It is ideal for applications where low stress is required. |
|
MasterSil 155 Two part, graphite filled silicone adhesive. Convenient one to one mix ratio by weight. Volume resistivity 20-40 ohm-cm. Elongatio >300%. Serviceable from -85°F to +400°F. |
|
MasterSil 323S-LO Addition curing, two part silicone for use as an adhesive, sealant, coating. Passes NASA low outgassing specifications. Serviceable from -80°F to +400°F. Electrically conductive with convenient processing. |
|
MasterSil 705C Single component, electrically conductive, non-corrosive silicone compound. Carbon filled. Tack free time 3-7 minutes at ambient temperatures. Paste viscosity. Serviceable up to 400°F. |
|
MasterSil 705S Silver filled, one-part, no-mix, non-corrosive silicone system. Shore A hardness 70. Cures at room temperatures when exposed to atmospheric moisture. Extremely low volume resistivity. Most effective when applied in thin sections. |
|
MasterSil 973S-LO Silver filled, two part, addition cured type silicone. Excellent electrical conductivity. Passes NASA low outgassing test requirements. Highly flexible. Service temperature range from -120°F to +400°F. Volume resistivit >0.004 ohm-cm. |