EP46HT-1AO Thermally conductive/electrically insulative heat resistant epoxy compound. Requires oven curing. Meets NASA low outgassing specifications. Meets MIL-STD-883J Section 3.5.2 for thermal stability. Excellent dimensional stability. Withstands 1,000 hours 85°C/85% RH. Serviceable from -100°F to +550°F. Tg 215-220°C. |
|
EP46HT-1ND-2 Heat resistant epoxy paste adhesive. Serviceable from -100°F to +600°F. Requires oven curing. Will not flow during processing. Superior electrical insulation and chemical resistant properties. Excellent mechanical strength. |
|
EP46HT-2 Serviceable from -100°F to +500°F. Tg 155-165°C. Superior durability. Heat curing, two component epoxy compound. Resists thermal cycling. Withstands 1,000 hours 85°C/85% RH. Good electrical insulator. Ability to protect against hostile chemical exposure. |
|
EP46HT-2AO Black Thermally conductive/electrically insulative. Passes NASA low outgassing tests. Serviceable from -100°F to +500°F. Tg 200-210°C. Remarkable dimensional stability. Impressive mechanical strength properties. |
|
EP46HT-2Med USP Class IV approved, heat resistant epoxy adhesive. Glass transition temperature in excess of 220°C. Withstands repeated exposure to autoclaving, radiation and chemical sterilants. High bond strength. Superior durability. Serviceable from -100°F to +500°F. Electrically insulative SUitable for potting. |
|
EP46HT-2ND2 Two part non-drip epoxy paste. Resists long term exposure from -100°F to +550°F. Superior peel strength. Protects against exposure to oils, fuels, hydrocarbons, acids, bases, solvents. Withstands thermal cycling and shock. |
|
EP48TC Ultra low thermal resistance properties. Can be applied in bond lines as thin as 10-15 microns. Low CTE. Low shrinkage upon cure. Passes NASA low outgassing testing. Serviceable from -100°F to +300°F. Exceptional dimensional stability. Withstands 1,000 hours 85°C/85% RH. |
|
EP4CL-80 One component, ultra low viscosity epoxy that offers thermal and electrical insulation and is optically clear. |
|
EP4CL-80Med One component, ultra low viscosity epoxy that offers thermal and electrical insulation and is optically clear. |
|
EP4EN-80 One component, low viscosity epoxy that offers thermal conductivity, electrical insulation and a filler material with ultra small particle sizes. This imparts high mechanical strength properties, outstanding dimensional stability and low shrinkage upon curing. |