Supreme 11HT-4 Two Part Epoxy Supreme 11HT-4

Two component, high strength epoxy adhesive. Serviceable for -100°F to +400°F. Excellent electrical insulation characteristics. Adheres well to similar/dissimilar substrates. Aramid fiber reinforcement for dimensional stability. Exceptional durability. 100 to 40 mix ratio by weight. Versatile cure schedules.

Supreme 11HT-LO Two Part Epoxy System Supreme 11HT-LO

Room temperature curing epoxy adhesive has a convenient one to one mix ratio. High shear and peel strength. Toughened. NASA low outgassing approved. Stress cracking fatigue resistant. Serviceable from -100°F to +400°F. Withstands 1,000 hours 85°C/85% RH. Fast setting. Good flow. Easy to apply.

Supreme 11HTLP Two Part Epoxy Supreme 11HTLP

High viscosity, two component, toughened epoxy adhesive/sealant. One to one mix ratio weight or volume. Favorable open time. Cure readily at room temperature. Outstanding toughness. High shear/peel strength. Resists impact, shock, thermal cycling. Serviceable from -100°F to +400°F.

Supreme 11HTLV Two Component Epoxy Supreme 11HTLV

High peel and shear strength system. Convenient one to one mix ratio. Serviceable from -100°F to +350°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. Readily machinable.

Supreme 11HTND Two Component Epoxy System Supreme 11HTND

High peel and shear strength system. Convenient one to one mix ratio with paste consistency. Serviceable from -112°F to +400°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability.

Two Part Epoxy Supreme 11LV Supreme 11LV

High peel and shear strength system. Convenient one to one mix ratio. Serviceable from -100°F to +250°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. Readily machinable.

One Part Epoxy System Supreme 17HT

Master Bond Supreme 17HT is a one component toughened epoxy for bonding and sealing. It has a moderate viscosity system with good flow properties.The service temperature range is from -100°F to +550°F.

Supreme 17HTMed

Master Bond Supreme 17HTMed is a one component toughened epoxy for bonding and sealing that meets ISO 10993-5 for biocompatibility. It has a moderate viscosity system with good flow properties.The service temperature range is from -100°F to +550°F.

Supreme 17HTND-2 One Component Epoxy Supreme 17HTND-2

Master Bond Supreme 17HTND-2 is a one component toughened epoxy for bonding and sealing. It is a paste system with good physical strength properties.The service temperature range is from -100°F to +550°F.

Supreme 3 One Part Epoxy Supreme 3

Storage stable one component heat curing epoxy adhesive. Versatile cure schedules. Electrically insulative. Durable system. Resists thermal cycling. Serviceable from -100°F to +250°F.