554 products match
LED401LV One part, low viscosity, optically clear system. Fast curing with a high bond strength. Superior dimensional stability and electrical insulative properties. Serviceable from -60°F to +250°F. |
|
LED403Med One part, high viscosity system. Cures tack-free without any oxygen inhibition. Meets USP Class VI specifications; also passes ISO 10993-5 cytotoxicity test. Resists gamma radiation, EtO and various chemical sterilants. Serviceable from -60°F to +250°F. |
|
LED405FL3 Fast cures under LED light. Outstanding optical clarity, with fluorescent dye. Can be used for small potting and encapsulation, as it can cure up to 1/8 inch thick. Withstands rigorous thermal cycling, mechanical shock and vibration. Serviceable from -100°F to +250°F. |
|
LED405Med One part, cures tack-free without any oxygen inhibition. Passes ISO 10993-5 cytotoxicity test. Serviceable from -60°F to +250°F. Superb optical clarity. |
|
LED415DC90 | |
LED415DC90Med | |
LED422DC90 | |
MasterSil 150 Two component, low viscosity condensation cured system. Used for potting and encapsulation. Superior toughness and resiliency. Protects against dust, moisture, ozone, thermal shock and vibration. Excellent thermal stability. Serviceable from -55°F to +400°F. |
|
MasterSil 151 Optically clear, addition curing potting, encapsulation, sealing compound. Low shrinkage upon cure. Resists up to +400°F [+204°C]. Shore A hardness 50-60. Highly resistant to water. Long pot life. |
|
MasterSil 151AO Thermally conductive silicone casting, potting and sealing system. Thermal conductivity of 0.35-.0.54 W/(m•K). Electrically isolating. Low viscosity system bonds well to a wide variety of substrates. Remarkable flexibility. Temperature resistant from -65°F to +400°F. White color. |