Master Bond Product Search

441 products match

Supreme 42HT-2ND-2 Two Component Epoxy Supreme 42HT-2ND-2

Two component, high temperature resistant epoxy adhesive, sealant, coating. Excellent toughness. Paste viscosity . Non-flowing even when heated. Gap filling. Superior thermal cycling capabilities. Chemical resistant. Service temperature range -80°F to +450°F.

Supreme 45HT Two Component Epoxy System Supreme 45HT

Toughened, thermally stable, two component epoxy adhesive, sealant, coating. Excellent peel strength. Superior thermal cycling capabilities. Withstands exposure to acids, bases, solvents, fuels, oils, water. Electrical insulator. Service temperature range -100°F to +450°F.

Master Bond Supreme 45HT-3 Epoxy System Supreme 45HT-3

Toughened, thermally stable, two component epoxy adhesive, sealant, coating. Excellent compressive strength. Abrasion resistant. Withstands exposure to acids, bases, solvents, fuels, oils, water. Electrical insulator. Service temperature range -100°F to +550°F.

Supreme 45HTND Two Part Epoxy Supreme 45HTND

Toughened, non-drip epoxy paste for bonding, sealing, coating. Serviceable from -100°F to +450°F. Two component system has long working life. Heat curing. High peel/shear strength properties. Withstands rigorous thermal cycling.

Supreme 45HTND-2 Two Part Epoxy Supreme 45HTND-2

Paste viscosity. Will not flow when cured. Gap filling. Serviceable from -100°F to +450°F. High peel and shear strength properties. Two part system. Long pot life. Good thermal cycling capabilities. Excellent electrical insulator.

Supreme 45HTND-2LO Black Two Part Epoxy Supreme 45HTND-2LO Black

Toughened, two component, non-drip epoxy paste. Service temperature range -100°F to +450°F. Long working life. Gap filling. Meets NASA low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superior electrical insulator. Heat curing.

Supreme 45HTQ Two Part Epoxy Compound Supreme 45HTQ

Two component, toughened, quartz filled epoxy with exceptional abrasion resistance. Heat curing system. Long working life after mixing. High compressive strength. Superb dimensional stability. Serviceable from -60°F to +450°F. Withstands exposure to petrochemicals acids, bases, solvents. Good strength retention at elevated temperatures. Successfully tested for 1,000 at 85°C/85% RH.

Supreme 45HTQ Two Component Epoxy Supreme 45HTQ-4

Toughened, two component silicon carbide filled epoxy. Heat curable. Exceptional abrasion and chemical resistance. Serviceable from -100°F to +450°F. Can withstand high compressive loads and rigorous thermal cycling. Good strength retention at elevated temperatures.

Two Part Epoxy System Supreme46HT-1AO Supreme 46HT-1AO

Toughened epoxy system, resists thermal cycling. Serviceable from -100°F to +500°F. Exceptionally long working life. Thermally conductive, electrically insulative.

Supreme 46HT-2 Two Part Epoxy Supreme 46HT-2

High strength epoxy adhesive. Outstanding toughness and durability. Serviceable from -100°F to +500°F. Withstand mechanical shocks and rigorous thermal cycling. Excellent peel strength. Cures at elevated temperature.