617 products match
MasterSil 711Med Exceptionally fast setting, high performance, non-corrosive silicone rubber. Used in medical device manufacturing. Has superb flexibility. Servicable from -75°F to +400°F. |
|
MasterSil 713 Easy to use, low viscosity, one part silicone compound. Superb elasticity. Non- corrosive. Ideal for small encapsulations and conformal coatings. Clear color. Fast tack-free time. Repairable. |
|
MasterSil 773 Ultra low viscosity silicone conformal coating material. Easily applied by spraying, brushing, dipping or flow coating. Superb humidity and heat resistance. |
|
MasterSil 800 Ultra high temperature resistance up to 300°C. Superb flexibility and elasticity. Non-corrosive. One component, room temperature curing. Flowable. |
|
MasterSil 800Med Ultra high temperature resistance up to 300°C. Superb flexibility and elasticity. Non-corrosive. One component, room temperature curing. Flowable. Meets ISO 10993-5 for non cytotoxicity. |
|
MasterSil 801 One component, silicone paste resists up to 300°C (572°F). Elongation 250-350%. Extremely soft. Non-corrosive cure. Available in tube, jar and cartridge containers. |
|
MasterSil 803 Unique non-corrosive neutral curing oxime type silicone featuring enhanced high and low temperature serviceability from -180°F up to +500°F(260°C). Features high bond strength and superior electrical insulation properties. Paste viscosity. |
|
MasterSil 910Med Acetoxy type system. Bonding, sealing, coating compound. Pass USP Class VI testing and ISO cytotoxicity specifications. Tack free time 10-20 minutes at 75°F. Shore A hardness 20-30. Elongation 400-600%. Paste viscosity. Service temperature range -75°F to +400°F. |
|
MasterSil 912Med Single component silicone with a paste viscosity for bonding, sealing and coating medical devices. Non-corrosive, neutral cure compound complies with USP Class VI and ISO 10993-5 specifications. Resists many kinds of sterilization including gamma and other types of radiation, EtO and some types of liquid sterilants. |
|
MasterSil 913Med Acetoxy type system. Bonding, sealing, coating compound. Pass ISO cytotoxicity specifications. Tack free time 10-20 minutes at 75°F. Shore A hardness 20-30. Elongation 600-700%. Paste viscosity. Service temperature range -75°F to +400°F. |