One component, high temperature resistant, electrically conductive, die attach epoxy

Key Features

  • Not premixed and frozen
  • Excellent dispensing profile
  • Meets MIL-STD 883J
  • NASA low outgassing

Product Description

Master Bond EP17HTS-DA is a one component, electrically conductive die attach epoxy featuring high temperature resistance. It is not premixed and frozen and has unlimited working life at room temperature. It has a paste consistency, and dispenses smoothly and easily, without any tailing. It can be applied either manually or with automated equipment. The system requires a 3 step curing schedule; cure for 1 hour at 180°F followed by 2-3 hours at 300°F with a post cure for 1-2 hours at 350°F. The recommended storage is in a refrigerator at 40°F to 50°F.

Upon curing, EP17HTS-DA has exceptional electrical conductivity and temperature resistance. The service temperature range extends from -80°F to +550°F. Especially noteworthy is its bond strength. This epoxy bonds well to metals, ceramics, silicon, and many other substrates. In fact, its lap shear strength exceeds other conductive epoxies by a minimum of 400-500 psi. Some other desirable properties include the ability to withstand thermal cycling as well as mechanical and thermal shocks. As a silver filled system, it is a superior heat conductor. EP17HTS-DA should be considered in die attach applications as well as in other situations where low volume resistivity and high temperature resistance is required. It is especially useful in microelectronic assemblies where most conductive, die attach adhesives lack adequate temperature resistance.

Product Advantages

  • Single component system; no mixing needed
  • Not premixed and frozen
  • Unlimited working life at room temperature
  • Superb dispensing profile for die attach applications
  • Notably high bond strength
  • Available in syringes for manual or automatic dispensing

Industrial Certifications


ASTM E595 Compliant

MIL-STD-883J for Thermal Stability

Meets EU Directive 2015/863

Packaging


Can

EP17HTS-DA is available is various sizes and units to accommodate customer's needs.

Request Information