EP21LVMed Product Information | MasterBond.com

Low viscosity, two component epoxy compound

EP21LVMed Two Part Epoxy System

Key Features

  • Meets USP Class VI certification
  • Passes ISO 10993-5 for cytotoxicity
  • Outstanding thermal cycling resistance
  • Cures at room temperature or elevated temperatures
  • Excellent chemical resistance
  • Serviceable from -65°F to +250°F