Two component, toughened epoxy for bonding and sealing with high temperature resistance
Key Features
- Easy processing
 - Paste consistency
 - NASA low outgassing
 - Withstands 1,000 hours 85°C/85% RH
 
Product Description
Master Bond epoxy system Supreme 33ND offers a highly attractive blend of superb physical strength properties, outstanding temperature resistance and easy handling along with a non-drip viscosity. The mix ratio is 100 to 70 by weight or 1 to 1 by volume. This non-flowable system bonds well to many different kinds of substrates including metals, composites, glass, ceramics, rubbers and plastics. t is cryogenically serviceable and has a wide temperature range extending from 4K up to +425°F. It is highly resistant to aggressive thermal cycling. It also has very good chemical resistance to water, fuels, hydraulics as well as many acids and bases. It is a solid electrical insulator with superior retention of those properties at elevated temperatures. Supreme 33ND has a number of curing options including cure schedules at room temperature, with heat or a combination of the two. The optimum cure is overnight at room temperature followed by a few hours at 150-200°F. Part A is colored gray and Part B is amber. Its exceptional dimensional stability and minimal shrinkage upon curing enables it to be an excellent choice for applications in the aerospace, electronic and specialty OEM industries.
Product Advantages
- Forgiving mix ratios: 100:70 by weight or 1:1 by volume
 - Bonds well to a wide variety of substrates
 - Cryogenically serviceable
 - Passes NASA low outgassing
 - Withstands 1,000 hours 85°C/85% RH
 
Industrial Certifications
Packaging
Supreme 33ND is available is various sizes and units to accommodate customer's needs.
			      