One component, B-stage epoxy for potting, encapsulation, coating and bonding

EP36AN One Component, B-stage Epoxy

Key Features

  • Toughened system
  • Excellent thermal conductivity
  • Superior electrical insulation properties
  • Resists up to +500°F
  • One part, B-stage system
  • Available in 30 gram cookies