Low viscosity, EP62-1LPSP is a two component epoxy that features an exceptionally long working life of 12-24 hours at ambient temperatures.
Two component, high performance epoxy system featuring convenient handling along with excellent temperature and chemical resistance
Key Features
- Exceptionally low viscosity
- Very long pot life at room temperature
- Fine optical clarity
- Cryogenically serviceable
- Meets NASA low outgassing specifications
- Withstands 1,000 hours 85°C/85% RH