MasterSil 151AO Product Information | MasterBond.com

Two part silicone for high performance casting, potting & encapsulation and sealing

MasterSil 151AO Two Part Silicone System

Key Features

  • Superior thermal conductivity
  • Low exotherm; very long pot life
  • Excellent flexibility
  • Superb electrical insulation properties
  • Can cure in thicknesses up to and beyond 1-2 inches
  • High temperatures resistance to +400°F