Our new video offers a look at MasterSil 930’s enhanced resistance to high temperature and a wide range of chemicals including fuels, oils and solvents.
One part, fluorosilicone system for high performance bonding, sealing & coating with enhanced chemical resistance
Key Features
- Paste consistency
- Longer open time
- Good physical strength profile
- Superior chemical resistance