One component, higher viscosity UV curable system for bonding, sealing and coating
Key Features
- Outstanding optical clarity
 - High glass transition temperature
 - Passes NASA low outgassing specifications
 - Withstands 1,000 hours 85°C/85% RH
 
Product Description
Master Bond UV10TK40 is a higher viscosity, one part UV system for bonding, sealing and coating with good optical clarity, excellent physical properties and a high glass transition temperature (Tg) of 135-140°C. UV10TK40 cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with 20-40 milliwatts per cm². The rate of cure depends upon the distance from the light source, the thickness of the section and the intensity of the light source. The system can cure in sections up to 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. Its chemical resistance is particularly good as it resists water, oils, acids, bases and solvents well. It is also an effective sealing and coating material. The system does not contain any solvents or diluents and none are released during cure. UV10TK40 combines low shrinkage with exceptional dimensional stability. UV10TK40 is an outstanding electrical insulator with a temperature range of -60°F to +450°F. It is effectively used for high production applications where fast fixture times and rapid curing are critical. UV10TK40 is best used in fiber-optic, o ptical, optoelectronic and electronic industries where high temperature resistance and higher viscosity are needed.
Product Advantages
- One component system
 - Moderate viscosity
 - Reliable electrical insulator
 - Adheres well to many substrates
 - Outstanding optical clarity; excellent light transmission
 - Meets NASA low outgassing specifications
 