One component, UV and heat curable epoxy compound with low to moderate viscosity

One Part UV and Heat Curable Compound

Key Features

  • Allows for curing in “shadowed out” areas
  • Cures at temperatures as low as 80°C
  • Convenient no mix system
  • Excellent physical strength properties