X5TC Product Information | MasterBond.com

One component, thermally conductive elastomeric system for high performance bonding and sealing

X5TC One Part Elastomeric System

Key Features

  • One part, no mix
  • Cures at room or elevated temperatures
  • Relatively fast curing
  • Good thermal conductivity