554 products match
EP5LTE-100 One component flowable epoxy for bonding and sealing applications. Unlimited working life. Low coefficient of thermal expansion. Non conductive. |
|
EP5TC-80 One component flowable paste epoxy for bonding, sealing and small encapsulation applications. High thermal conductivity and electrical insulation properties. Ultra fine particles filler material that allows application in very thin sections. Low exotherm and great dimensional stability. Serviceable from -50°C to +150°C. |
|
EP62-1 Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. |
|
EP62-1AO Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. |
|
EP62-1BF Cures rapidly at moderate elevated temperatures. Superior resistance to harsh chemicals. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +500°F. Tg 170-175°C. Shore D hardness 80-90. |
|
EP62-1HT Superior resistance to harsh chemicals, particularly to acids. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-160°C. Shore D hardness 80-90. |
|
EP62-1HTMed Black Superior sterilization resistance. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-155°C. Shore D hardness 80-90. |
|
EP62-1HTMed Superior sterilization resistance. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-155°C. Shore D hardness 80-90. |
|
EP62-1LO Long working life. Cures quickly at moderate temperatures. Passes NASA low outgassing requirements. T >170°C. Resists exposure to acids, bases, many solvents and other chemicals. Superior bond strength properties. Service operating temperature range from -60°F to +450°F. |
|
EP62-1LPSP Low viscosity, optically clear epoxy with superior electrical insulation properties. Thermal stability. Exceptional chemical resistance. Long working life. Low exotherm. Withstands 1,000 hours 85°C/85% RH. Meets NASA low outgassing specifications. Serviceable from 4K to +400°F. |